ChevronTexaco TC-W3 2-Cycle Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco TC-W3 2-Cycle Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesChevron 2-Cycle Oil TC-W3 is a high quality two-stoke engine lubricant that delivers excellent performance in water-cooled and air-cooled applications. It is formulated to provide excellent lubrication and deposit control in a wide range of applications.Chevron 2-Cycle Oil TC-W3 contains a special ashless detergent designed to minimize piston rings from sticking to keep the engine operating smoothly and efficiently. Chevron 2-Cylce Oil TC W3 will keep the engine clean of deposits and will also protect the pistons from scuffing and pre-ignition problems.To enhance storage and transportation safety, Chevron 2-Cycle Oil TC-W3 contains a high flash solvent. This solvent also allows good mixing with gasoline at very low temperatures.It is dyed teal blue for easy identification of fuel-oil mixtures in pre-mixed applications.ApplicationsChevron 2-Cycle Oil TC-W3 is recommended as a premium lubricant for use in two-stroke engines where the latest TC-W3 or earlier general purpose lubricants are recommended. There applications include outboard engines, snowmobiles, motorcycles, lawn mowers, scooters, golf carts, chain saws, and other two-stroke powered equipments.Chevron 2-Cylce Oil TC-W3 is well suited for engines using oil injection systems with fuel/oil mixture ratios of up to 150:1.Chevron 2-cycle Oil TC W3 has excellent low temperature mixing characteristics that make It very suitable for use in cold climate conditions.
Physical Properties Metric English Comments
API Gravity 31.4 °
31.4 °
Brookfield Viscosity 5500 cP

@Temperature -25.0 °C
5500 cP

@Temperature -13.0 °F
Viscosity Measurement 119
119
Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 46.5 cSt
46.5 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.3 cSt
7.3 cSt
ASTM D445
Ash 0.00 %
0.00 %
Sulfated Ash wt%
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
ASTM D97
Flash Point 95.0 °C
203 °F
ASTM D92
Chemical Properties Metric English Comments
Total Base Number 3.8
3.8
ASTM D2896