Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass fabricThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Layer 1, Silicone Property; Arlon SQA-TMS-024
1.35 g/cc
0.0488 lb/in³
Layer 2, Silicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Interleave
165 microns
6.50 mil
Layer 1; Arlon SQA-TMS-003
267 microns
10.5 mil
Layer 2; Arlon SQA-TMS-003
406 microns
16.0 mil
Substrate; Arlon SQA-TMS-003
838 microns
33.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Layer 1, Silicone Property; ASTM D2240
60
60
Layer 2, Silicone Property; ASTM D2240
Tensile Strength 5.52 MPa
800 psi
Layer 1, Silicone Property; ASTM D412
5.52 MPa
800 psi
Layer 2, Silicone Property; ASTM D412
Elongation at Break 225 %
225 %
Layer 1, Silicone Property; ASTM D412
225 %
225 %
Layer 2, Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Layer 1, Die B, Silicone Property; ASTM D624
15.8 kN/m
90.0 pli
[ppiw], Layer 2, Die B, Silicone Property; ASTM D624
Peel Strength 2.33 kN/m
13.3 pli
(S1 to S1), Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
UL RTI, Electrical 220 °C
428 °F
E54153
UL RTI, Mechanical without Impact 220 °C
428 °F
E54153
Electrical Properties Metric English Comments
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 34.5
Arlon SQA-TMS-025