Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Polyethylene Interleave
127 microns
5.00 mil
Kodacel Carrier
584 - 686 microns
23.0 - 27.0 mil
Overall
584 - 686 microns
23.0 - 27.0 mil
Side 1
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Compound Property
Tensile Strength >= 6.21 MPa
>= 900 psi
Compound Property
Elongation at Break >= 300 %
>= 300 %
Compound Property
Peel Strength >= 1.05 kN/m
>= 6.00 pli
Bond Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
rated per UL card E54153
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 22.7 - 26.7
Users viewing this material also viewed the following: