| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. ..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
|
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. ..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Thickness | 635 - 686 microns | 25.0 - 27.0 mil | Overall |
|
Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Semi-Cured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications...
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
|
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
|
|||
| Thickness | 660 - 686 microns | 26.0 - 27.0 mil | Overall |
|
Arlon 56581R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. T..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 30580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
|
Arlon 30580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
|
Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 44570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
|
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier
(discontinued **)&
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data ..
|
|||
| Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
|
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier
(discontinued **)&
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data ..
|
|||