| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 356 microns | 14.0 mil | |
|
Polystrand ThermoBallistic™ TBE8010X X-Ply Cross-Ply Polypropylene-Glass Composite
2-Ply with Fiber Orientation at 0° & 90°.. Polystrand ThermoBallistic laminates combine continuous E-Glass (ThermoBallistic-E™) structural fibers with a proprietary polypropylene thermoplastic po..
|
|||
| Thickness | 356 microns | 14.0 mil | Per Ply |
|
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K 8HS Carbon Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
|
|||
| Thickness | 356 - 1270 microns | 14.0 - 50.0 mil | |
|
Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi..
|
|||
| Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R35551X014 0.014" (0.356 mm) Uncured Rubber with Coated Nextel Substrate
(discontinued **)
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberSubstrate: Coated Nextel This data Represents typical values for the production material. The data should not be used to write, or in ..
|
|||
| Thickness | 356 microns | 14.0 mil | Typical; ASTM D374 |
|
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
|
Arlon 19562R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr..
|
|||
| Thickness | 356 microns | 14.0 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Cured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
|
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
|
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat..
|
|||
| Thickness | 356 microns | 14.0 mil | Substrate; Arlon SQA-TMS-003 |
|
Arlon 19606R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: 0.003" PolyethyleneThis data represents typical values for the ..
|
|||
| Thickness | 356 microns | 14.0 mil | substrate; Arlon SQA-TMS-003 |
|
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate
Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene
|
|||
| Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
|
Arlon 28561R015M 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. T..
|
|||
| Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
|
Arlon 30560R015 0.015" (0.381 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier
Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The..
|
|||
| Thickness | 356 microns | 14.0 mil | Layer 1; Arlon SQA-TMS-003 |
|
Arlon 61089R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Denier Vectran HS Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 1000 Denier HS Appearance: Red silicone gum on fabricThis data represents t..
|
|||
| Thickness | 356 microns | 14.0 mil | Nominal |
|
AK Steel CARLITE® M-6 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
|
|||
| Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
|
Arlon P29609R015 0.015" (0.381 mm) Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr..
|
|||
| Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R34381R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 7628 Style FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typical..
|
|||
| Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R34581R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 7628 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents ty..
|
|||
| Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber
Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 2116 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicon..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 11523 Fiberglass, Substrate |
|
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 1523 Fiberglass, Substrate |
|
Arlon 19096R022 0.022" (0.559 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place of,..
|
|||
| Thickness | 356 - 406 microns | 14.0 - 16.0 mil | Overall |
|
Arlon 51946C015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Thickness | 356 microns | 14.0 mil | substrate; Arlon SQA-TMS-003 |
|
Arlon 53423R032 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: cured silicone rubber
|
|||
| Thickness | 356 microns | 14.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
|
Arlon 54331R014 0.014" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: Blue LDPESide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Blue LDPEThis data represents typical valu..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 2523 Fiberglass, Substrate |
|
Arlon R31246R060 0.060" (1.52 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 2523 Fiberglass, Substrate |
|
Arlon R31246R063 0.063" (1.60 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate..
|
|||
| Thickness | 356 microns | 14.0 mil | Prime Coated 2523 Fiberglass, Substrate |
|
Arlon R34256R063 0.063" ((1.60 mm) Uncured/Cured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate..
|
|||
| Thickness | 356 - 457 microns | 14.0 - 18.0 mil | Caliper |
|
3M Diamond Grade™ 983 Conspicuity Markings
3M™ Diamond Grade™ Conspicuity Markings Series 983 are highly retrorflective micro-prismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detection. The ref..
|
|||
| Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R36461R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Liner: Polyethylene This data represents typical values for..
|
|||
| Thickness | 356 microns | 14.0 mil | Overall; Arlon SQA-TMS-003 |
|
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber
Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib..
|
|||