Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.30 - 1.32 g/cc @Temperature 25.0 °C |
1.30 - 1.32 g/cc @Temperature 77.0 °F |
|
Oceanchem Group Resorcinol bis (Diphenyl Phosphate) (RDP) Molecular Formula: C30H24O8P2Cas No.: 57583-54-7RDP is a halogen-free phosphorus-based flame retardant.Use:RDP flame retardant provides a halogen-free solution for flame retarding PC/ABS, PPO/HIPS a.. |
|||
Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D792 |
S&E Specialty Polymers GA-2285FR PVC Application: 80°C clear flame retardant PVC compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D792 |
S&E Specialty Polymers GTPO8290-GT7 PVC Application: 80°C, Low Smoke, Zero Halogen, Flame Retardant Polyethylene Compound for extrusion applications. Specifically designed to withstand severe UV exposure while maintaining very good .. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D 792 |
Karina E CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax CCP PBT 1100-211X Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1100-211H Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1100-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1100-211S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
Karina 40/418-FC-LMP Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D 792 |
Karina 501D48/1-D-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
Karina E 40/25-FC-LMP Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
Karina E 701D02/128-SD Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
Karina E 750-35/2-IS-SD-TR-LMP Ivory PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | NBR NM-IEC 60811-1-3 |
Karina 600D48/1-C-IS Black PVC Compound PVC Compound recommended for injection of automotive parts and extrusion of flexible jacket for electrical cablesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.26 - 1.32 g/cc | 1.26 - 1.32 g/cc | ASTM D 792 |
Karina E 880-10/136-A-IS-As White PVC Compound Anti-UV and anti-fungus additivated PVC compound, recommended for general extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom C-550170 PVC Description: Compuestos Dominicanos, S.A. produces a wide variety of PVC compounds for the injection molding of foot wear products, everything from full injection, shoe soles, boots, and PVC compoun.. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
Axiall 14820 Wire & Cable Flexible PVC Non-lead stabilized drop cable jacketing. Also suitable for 80C rated general purpose jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
Axiall 830B Wire & Cable Flexible PVC 80°C rated compound recommended for UL 360, liquid tight flexible conduit jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
Axiall 8940 Moldings & Extrusions Flexible PVC General purpose semi-rigid extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Adamas Rixon U PEEK, Unreinforced Information provided by Adamas, HPM |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
Axiall 10705 Wire & Cable Flexible PVC Non-lead stabilized general purpose 75C compound with good low temperature properties. Formulated for increased line speed and reduced surface gloss.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
Axiall 38511 Wire & Cable Flexible PVC Tray cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.28 - 1.32 g/cc | 1.28 - 1.32 g/cc | ASTM D-792 |
Axiall 4501 Flexible PVC Non-lead stabilized, 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1100-211MB Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Specific Gravity | 1.30 - 1.32 g/cc | 1.30 - 1.32 g/cc | ASTM D792 |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |