Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.011 cm/cm | 0.011 in/in | MD; ASTM D955 |
Melt Flow | 12 g/10 min | 12 g/10 min | ASTM D1238 |
Ash | 10 % | 10 % | ASTM D2584 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 89 | 89 | ASTM D785 |
Tensile Strength at Break | 25.0 MPa | 3630 psi | ASTM D638 |
Tensile Strength, Yield | 34.0 MPa | 4930 psi | ASTM D638 |
Elongation at Break | 25 % | 25 % | ASTM D638 |
Elongation at Yield | 7.0 % | 7.0 % | ASTM D638 |
Tensile Modulus | 1.60 GPa | 232 ksi | ASTM D638 |
Flexural Strength | 37.0 MPa | 5370 psi | ASTM D790 |
Flexural Modulus | 1.500 GPa | 217.5 ksi | ASTM D790 |
Izod Impact, Notched | 0.438 J/cm | 0.820 ft-lb/in | ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 226 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 61.1 °C | 142 °F |