Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON NV003E PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* VERTON* NV003E is a compound based on PC+ABS Blend resin containing 15% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 112 MPa
16200 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ISO 527
Tensile Modulus 5.77 GPa
837 ksi
1 mm/min; ISO 527
Flexural Strength 162 MPa
23500 psi
ISO 178
Flexural Modulus 5.68 GPa
824 ksi
ISO 178
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
23.0 kJ/m²

@Temperature -40.0 °C
10.9 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Dart Drop, Total Energy 18.0 J
13.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af