Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO SEAL SERIES
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TURBO SEAL SERIES 85 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The high lubricating properties of this compound prevent galling on stainless steel, aluminum and all other metal pipe threads and fittings.UL Classification Classified as small fire hazard. No flash point in liquid state. Ignition temperature 465°C. For use in devices handling gasoline, petroleum oils, natural gas, propane and butane.Applications: Recommended for industrial applications in the chemical processing, petroleum refining, pulp/paper, waste treatment, textile, utilities/power generation, marine, automotive, industrial equipment, gas compression and distribution industries.Widely used for industrial plant fluid power systems.Part Numbers for this data: 85-051Information provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Brookfield Viscosity 540000 cP
540000 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength >= 1.00 MPa
>= 145 psi
Steel Pins & Collars; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point >= 37.8 °C
>= 100 °F
Processing Properties Metric English Comments
Cure Time 120 - 240 min
2.00 - 4.00 hour
Functional
1440 min
24.0 hour
Full
10.0 - 30.0 min

@Temperature -65.0 - 400 °C
0.167 - 0.500 hour

@Temperature -85.0 - 752 °F
Handling
Descriptive Properties Value Comments
Appearance White
Chemical Resistance 100% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
60% Initial Strength Retained
Acetone at 22°C, at 1000hrs
70% Initial Strength Retained
Acetone at 22°C, at 500hrs
75% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
75% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
80% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
80% Initial Strength Retained
Gasoline at 22°C, at 500hrs
90% Initial Strength Retained
Ethanol at 22°C, at 500hrs
90% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
95% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
Composition Methacrylate ester
Operation Pressure 10000 psi
Torque >1.7 N.m
Breakaway, M10 steel nuts and bolts, ISO 10964
1 N.m
Prevail, M10 steel nuts and bolts, ISO 10964
Users viewing this material also viewed the following: