| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183-A |
|
Okulen® 500 - REG PE Multicoloured coarse
OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel..
|
|||
| Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
|
SABIC B4660/B4660AB High Density Polyethylene for Blow Molding
Product Description: B4660 series grades are medium molecular weight High Density Polyethylene homopolymer for blow molding applications. They are primarily designed for imparting high rigidity, t..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPH TS15010 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
|
Quadrant EPP Cestilene™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | TA4820B |
|
Permabond TA4820 Structural Acrylic Adhesive
PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | |
|
Mitsui Fybrel® E 795 Polyolefin Synthetic Pulp, Dry Processes
(discontinued **)
Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type ..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D-792 |
|
Polyram BondyRam® 2001 Maleic Anhydride modified EVA coupling agent
(discontinued **)
Maleic Anhydride Modified grafted EVA (28%VA) recommended as adhesive promoter and general purpose compatibilizerInformation provided by Polyram Ram On Ind.
|
|||
| Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D4883 |
|
Ineos T60-500 HDPE
T60-500 is a high density polyethylene homopolymer designed specifically for injection molding. This narrow molecular weight distribution resin is a product of Ineos USA, LLC's innovative technolog..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | |
|
JPJ Technologies 5200B HDPE Blow Molding
Information provided by JPJ Technologies
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | |
|
Solvay ALKAQUAT® DMB-451 80% Surfactant
Identification: Alkyl Dimethyl Benzyl Ammonium ChlorideCAS: 68424-85-1 Water Solubility: SolubleAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAQUAT© DMB-451 ..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
|
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
|
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
|
Unipetrol PE HD LITEN® MB/ML 62 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | |
|
Goodfellow Polyethylene Fiber/Polyethylene composite
Information provided by Goodfellow.
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1505 |
|
CPC - Vycom HITEC® HDPE High Density Polyethylene
Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1505 |
|
CPC - Vycom SANATEC® Sanitary Cutting Boards High Density Polyethylene
Sanatec is a high density polyethylene specially formulated for the manufacture of quality cutting boards. Sanatec`s special surface finish insures long product life and will not dull knives. Sanate..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | |
|
Dow HDPE 30460M High Density Polyethylene
DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | |
|
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
|
|||
| Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D792 |
|
Aclo Accutech Polypropylene Homopolymer HP0339C10L Calcium Reinforced |
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 2781 |
|
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1505 |
|
Amco PRIMATOP HDPE 080960 Injection Molding Polyethylene
HDPE 080960 features high stiffness, maximum toughness, good top loading capability, and high surface gloss. Applications include tote boxes and beverage crates.Former A-Top Polymers product; part o..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
|
CENTROPLAST CENTROLEN PE-HD Polyethylene high density
This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor..
|
|||
| Density |
0.960
-
1.02
g/cc <br>@Temperature 280 - 330 °C
|
0.0347
-
0.0368
lb/in³ <br>@Temperature 536 - 626 °F
|
Average value: 1.01 g/cc Grade Count:43 |
|
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Density | 0.960 - 11.0 g/cc | 0.0347 - 0.397 lb/in³ | Average value: 1.26 g/cc Grade Count:92 |
|
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
|
LyondellBasell Hifax™ HSBMF248 Thermoplastic Polyolefin Elastomer
Description: Hifax™ HSBMF248 high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of flow, rigidity, low t..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183/A |
|
Addiplast Addilene PMD 50265 Flame Retardant Polypropylene
Flame retardant, high rigidityInformation provided by Addiplast.
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON MS000IL PP
LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c..
|
|||
| Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP STAT-KON MS000IL PP
LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c..
|
|||