Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories A40 Special High-Density Gunning Castable

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chosun Refractories A40 Special High-Density Gunning Castable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.18 g/cc
<br>@Temperature 1000 °C,<br> Time 10800 sec
0.0788 lb/in³
<br>@Temperature 1830 °F,<br> Time 3.00 hour
2.18 g/cc
<br>@Temperature 1350 °C,<br> Time 10800 sec
0.0788 lb/in³
<br>@Temperature 2460 °F,<br> Time 3.00 hour
2.21 g/cc
<br>@Temperature 110 °C,<br> Time 86400 sec
0.0798 lb/in³
<br>@Temperature 230 °F,<br> Time 24.0 hour
Porosity 18 %
<br>@Temperature 110 °C,<br> Time 86400 sec
18 %
<br>@Temperature 230 °F,<br> Time 24.0 hour
22 %
<br>@Temperature 1350 °C,<br> Time 10800 sec
22 %
<br>@Temperature 2460 °F,<br> Time 3.00 hour
22.5 %
<br>@Temperature 1000 °C,<br> Time 10800 sec
22.5 %
<br>@Temperature 1830 °F,<br> Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.008829 GPa
<br>@Temperature 110 °C,<br> Time 86400 sec
1.281 ksi
<br>@Temperature 230 °F,<br> Time 24.0 hour
0.00981 GPa
<br>@Temperature 1000 °C,<br> Time 10800 sec
1.42 ksi
<br>@Temperature 1830 °F,<br> Time 3.00 hour
0.012753 GPa
<br>@Temperature 1350 °C,<br> Time 10800 sec
1.8497 ksi
<br>@Temperature 2460 °F,<br> Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.100 %
<br>@Temperature 1000 °C,<br> Time 10800 sec
-0.100 %
<br>@Temperature 1830 °F,<br> Time 3.00 hour
-0.0600 %
<br>@Temperature 110 °C,<br> Time 86400 sec
-0.0600 %
<br>@Temperature 230 °F,<br> Time 24.0 hour
0.050 %
<br>@Temperature 1350 °C,<br> Time 10800 sec
0.050 %
<br>@Temperature 2460 °F,<br> Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
SiO2 45 %
45 %
Descriptive Properties Value Comments
Main Applications Blast furnace shaft
Material Required for Estimating (kg/?) 2,300
Copyright © lookpolymers.com All Rights Reserved