Denka CL-430 Transparent Resin Polymer (MABS) ABS |
ABS Polymer |
|
Denka LCS Z1050 Thermoplastic Elastomer, Extrusion grade (general) |
Elastomer, TPE |
LCS
|
Denka LCS Z1060 Thermoplastic Elastomer, Extrusion grade (general) |
Elastomer, TPE |
LCS
|
Denka LCS Z1070 Thermoplastic Elastomer, Extrusion grade (general) |
Elastomer, TPE |
LCS
|
Denka LCS Z1075 Thermoplastic Elastomer, Extrusion grade (general) |
Elastomer, TPE |
LCS
|
Denka LCS Z6050 Thermoplastic Elastomer, Injection Molding Grade (general) |
Elastomer, TPE |
LCS
|
Denka LCS Z6070 Thermoplastic Elastomer, Injection Molding Grade (general) |
Elastomer, TPE |
LCS
|
Denka MALECCA K-090 ABS |
ABS Polymer |
MALECCA
|
Denka MALECCA K-095 ABS |
ABS Polymer |
MALECCA
|
Denka MALECCA K-100 ABS |
ABS Polymer |
MALECCA
|
Denka MALECCA K-200 ABS |
ABS Polymer |
MALECCA
|
Denka MALECCA K-300 ABS |
ABS Polymer |
MALECCA
|
Denka MALECCA K-400 ABS |
ABS Polymer |
MALECCA
|
Denka MALECCA K-510 ABS |
ABS Polymer |
MALECCA
|
Denka MALECCA K-700 ABS |
ABS Polymer |
MALECCA
|
Denka REOMER G G3000 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G3010 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G3012 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G3021 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G3070 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5048 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5059 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5072 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5074 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5082 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5369 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5377 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5379 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G5479 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G8053 Thermoplastic Elastomer, For Injection Molding |
Elastomer, TPE |
|
Denka REOMER G G8070 Thermoplastic Elastomer, For Injection Molding |
Elastomer, TPE |
|
Denka REOMER G G8082 Thermoplastic Elastomer, For Injection Molding |
Elastomer, TPE |
|
Denka REOMER G G8250 Thermoplastic Elastomer, For Injection Molding |
Elastomer, TPE |
|
Denka REOMER G G8355 Thermoplastic Elastomer, For Injection Molding |
Elastomer, TPE |
|
Denka STYROL MW1 Polystyrene |
Polystyrene, Molded, Unreinforced |
STYROL
|
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS |
ABS Polymer |
|
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS |
ABS Polymer |
|
Denka TE-30 Transparent Resin Polymer (MABS resin) ABS |
ABS Polymer |
|
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene |
Styrene-Butadiene |
|
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene |
Styrene-Butadiene |
|
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene |
Styrene-Butadiene |
|
Denka TP-801 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene |
Styrene-Butadiene |
|
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene |
Styrene-Butadiene |
|
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene |
Styrene-Butadiene |
|
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene |
Thermoplastic |
|
Denka VINYKON G5070 PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON G5369 PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M1022A PVC, M grade for hard injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M1071 PVC, M grade for hard injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M1600 PVC, M grade for hard injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M2026 PVC, M grade for hard injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M2510 PVC, M grade for soft injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M4000 PVC, M grade for hard injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M557050 PVC, M grade for soft injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M558070 PVC, M grade for soft injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M7100 PVC, M grade for soft injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON M7300 PVC, M grade for soft injection molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON R2001 PVC, R grade for hard extrusion |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON R2015 PVC, R grade for hard extrusion |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON R3105 PVC, R grade for hard extrusion |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON R3201 PVC, R grade for hard extrusion |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON R4105 PVC, R grade for hard extrusion |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON R5020 PVC, R grade for hard extrusion |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S210040 PVC, S grade for transparent extrusion molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S210070 PVC, S grade for transparent extrusion molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S210075 PVC, S grade for transparent extrusion molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S210085 PVC, S grade for transparent extrusion molding |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S3029 PVC, S grade for window frame gaskets |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S3029A PVC, S grade for window frame gaskets |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S3095K PVC, S grade for refrigerator gaskets |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S3097 PVC, S grade for refrigerator gaskets |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON S3098 PVC, S grade for refrigerator gaskets |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON TS1007T PVC, S grade for window frame gaskets |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W1021 PVC, W grade for insulation, for sheaths |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W1022 PVC, W grade for insulation, for sheaths |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W1051 PVC, W grade for insulation, for sheaths |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W1080 PVC, W grade for insulation, for sheaths |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W2035 PVC, W grade for insulation, for sheaths |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W2085 PVC, W grade for insulation, for sheaths |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W2086 PVC, W grade for insulation, for sheaths |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W3012 PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W3050 PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W4023A PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W4029 PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W4050 PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W4200 PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W4203 PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W4800 PVC, W grade for equipment cords, for heat resistance |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W5120 PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W5230 PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W5520 PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W7080 PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W7100i PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W7100N PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka VINYKON W7300E PVC, W grade for non-migratory sheath and special items |
Vinyl (PVC) |
VINYKON
|
Denka LCS Z6060 Thermoplastic Elastomer, Injection Molding Grade (general) |
Elastomer, TPE |
LCS
|
Denka MALECCA K-600 ABS |
ABS Polymer |
MALECCA
|
Denka REOMER G G3015 Thermoplastic Elastomer, For Extrusion |
Elastomer, TPE |
|
Denka REOMER G G8354 Thermoplastic Elastomer, For Injection Molding |
Elastomer, TPE |
|
Denka TX-600S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene |
Thermoplastic |
|