Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Denka VINYKON W3050 PVC, W grade for equipment cords, for heat resistance

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON W3050 PVC, W grade for equipment cords, for heat resistance.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.422 g/cc
0.05137 lb/in³
JIS-Z-8807
Deformation 9.0 %
9.0 %
JIS-K-6723
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
JIS-K-6301
Tensile Strength at Break 17.658 MPa
2561.1 psi
JIS-K-6723
Elongation at Break 350 %
350 %
JIS-K-6723
100% Modulus 0.00981 GPa
1.42 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -31.0 °C
-23.8 °F
JIS-K-6723
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+12 ohm-cm

@Temperature 60.0 °C
7.00e+12 ohm-cm

@Temperature 140 °F
JIS-K-6723
2.00e+13 ohm-cm

@Temperature 30.0 °C
2.00e+13 ohm-cm

@Temperature 86.0 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 92
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 100
JIS-A-5756
Oil Resistance: Retention of Tensile Strength, % 93
JIS-K-6723
Oil Resistance: Retention Rate of Elongation, % 80
JIS-K-6723
Thermostability, min, JIS-K-6723 >240