Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.267 g/cc
0.04577 lb/in³
JIS-Z-8807
Deformation 15 %
15 %
JIS-K-6723
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
JIS-K-6301
Tensile Strength at Break 17.658 MPa
2561.1 psi
JIS-K-6723
Elongation at Break 380 %
380 %
JIS-K-6723
100% Modulus 0.005886 GPa
0.8537 ksi
JIS-K-6723
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -47.0 °C
-52.6 °F
JIS-K-6723
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm

@Temperature 30.0 °C
1.00e+11 ohm-cm

@Temperature 86.0 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 94
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 94
JIS-A-5756
Oil Resistance: Retention of Tensile Strength, % 95
JIS-K-6723
Oil Resistance: Retention Rate of Elongation, % 80
JIS-K-6723
Thermostability, min, JIS-K-6723 >240