Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | Cond. A; IPC 2.5.17.1 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 85GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 85U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm @Temperature 25.0 °C |
1.20e+16 ohm-cm @Temperature 77.0 °F |
|
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Volume Resistivity | >= 1.20e+16 ohm-cm | >= 1.20e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Valox® 357 PBT PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 1.20e+16 ohm-cm | >= 1.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Volume Resistivity | >= 1.20e+16 ohm-cm | >= 1.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Volume Resistivity | >= 1.20e+16 ohm-cm | >= 1.20e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Volume Resistivity | >= 1.20e+16 ohm-cm | >= 1.20e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Valox® 357U PBT Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 1.20e+16 ohm-cm | >= 1.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Volume Resistivity | >= 1.20e+16 ohm-cm | >= 1.20e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 357U PBT+PC Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm @Thickness 2.00 mm |
1.20e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT 403 M-G20 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | ASTM D257 |
BLUESTAR 403G-MG20 PBT, 20% Glass Filled Typical Applications: High GWIT, RTI, E/EInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 1.20e+16 ohm-cm @Thickness 2.00 mm |
1.20e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G20 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm @Thickness 2.00 mm |
1.20e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G20 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm @Thickness 2.00 mm |
1.20e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G20 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm @Thickness 2.00 mm |
1.20e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | ASTM D257 |
BLUESTAR 201-G20202 PBT, 20% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Volume Resistivity | 1.20e+16 ohm-cm | 1.20e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |