Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP324E Clear Two Part Epoxy Casting Resin Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP965LVLX Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF/M15 HS L BK 40/15% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 15% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF/M40 IG BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm @Temperature 20.0 °C |
8.00e+14 ohm-cm @Temperature 68.0 °F |
BS 2782 |
Teknor Apex Sinvicomp SIH 6007A Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Wire and Cable Applications Wire Types: V-90 Agency Ratings: AS 3147-1992 Forms: Pellets Processing Method: ExtrusionInformation Provided by.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Volume Resistivity | 8.00e+14 ohm-cm @Temperature 20.0 °C |
8.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 018/15 Halogen Free PVC General purpose |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP965LVLX Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965LVLX Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has .. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |
|||
Volume Resistivity | 8.00e+14 ohm-cm | 8.00e+14 ohm-cm | |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |