Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | 40 hours; 23C; 50% RH; ASTM D257 |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | after 40 hours at 23°C, 50% RH; ASTM D257 |
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | after 40 hours at 23°C, 50% RH; ASTM D257 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | |
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | |
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | |
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm @Temperature 65.0 °C |
6.00e+15 ohm-cm @Temperature 149 °F |
|
Tra-Con Tra-Cast FS407 Low Viscosity High Temperature Epoxy Casting System TRA-CAST FS407 is a low viscosity, solvent-free epoxy casting system recommended for rigid industrial laminating, electrical potting and transformer or coil embedding applications that require the e.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3105A Polybutylene Terephthalate (PBT), Epoxy adhesion improved, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | |
Tra-Con Tra-Bond 2101 General Purpose Epoxy Adhesive TRA-BOND 2101 is a medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of its superior structural, mechanical and ele.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC) Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh.. |
|||
Volume Resistivity | <= 6.00e+15 ohm-cm | <= 6.00e+15 ohm-cm | |
Cytec (Conap) FR-1046 / EA-02 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LDPE LD 150BW Wire & Cable Low Density Polyethylene Resin Product Description: LD 150BW is a LDPE containing suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house compounding it can a.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LDPE LD 157CW Wire & Cable Low Density Polyethylene Resin Product Description: LD 157CW is a medium density LDPE recommended for the production of Low Voltage power cable insulation, using the on-step silane cross0linking technology. The grade contains a h.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 4004EL Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 4004EL is a C4 Ziegler Natta LLDPE, especially designed for Low Voltage power cable insulation, using the two-step silane cross-linking process. Sufficient Cu-inhibitor shoul.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | ASTM D257 |
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Volume Resistivity | 6.00e+15 ohm-cm @Thickness 3.00 mm |
6.00e+15 ohm-cm @Thickness 0.118 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm @Thickness 3.00 mm |
6.00e+15 ohm-cm @Thickness 0.118 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Volume Resistivity | 6.00e+15 ohm-cm | 6.00e+15 ohm-cm | |
Atom Adhesives AA-BOND 2101 Epoxy Adhesive AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and el.. |