Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
Ineos ABS Lustran® H702 Medium heat resistance, increased flow. ,Property data per ISO test methods. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel.. |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 1.00 mm |
914 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® SF810 Polycarbonate, Glass Fiber Reinforced Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Structural foam• 10%.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610 Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 3817 black 9992 PA12 Product description: Grilamid XE 3817 black 9992 is a medium viscosity, heat and UV-stabilized Polyamid 12. Grilamid XE 3817 black 9992 is especially suitable for the coating of metal tubes and offe.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
Arkema Group Orgalloy® R 6600 Nylon 66 Alloy, Rigid Grade (Conditioned) Rigid polyamide 6.6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
Arkema Group Orgalloy® RS 6010 Nylon 6 Alloy, 10% Glass Fiber Reinforced (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 1.00 mm |
914 kV/in @Thickness 0.0394 in |
ASTM D149 |
Arkema Group Orgalloy® RS 6620 Polyamide 6.6 Alloy 20% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Petra® 110 BK-112 15% Glass Filled PET Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | IEC 60243-1 |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |
|||
Dielectric Strength | 36.0 kV/mm | 914 kV/in | |
Arkema Group Orgalloy® LT 5050T Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |