| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 60% Glass Fiber Filled |
| Manufacturer | EMS-Grivory (EMS-CHEMIE) |
| Trade Name | Grivory® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | EMS-Grivory Grivory® BG-60 FC PA6-GF60.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
| Water Absorption | 4.2 % | 4.2 % | ISO 62 |
| Moisture Absorption | 1.10 % | 1.10 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | ISO 294-4, 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 156 MPa | 22600 psi | conditioned; ISO 2039-1 |
| 273 MPa | 39600 psi | dry; ISO 2039-1 | |
| Tensile Strength at Break | 160 MPa | 23200 psi | conditioned; ISO 527-1/-2 |
| 245 MPa | 35500 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 3.2 % | 3.2 % | dry; ISO 527-1/-2 |
| 3.4 % | 3.4 % | conditioned; ISO 527-1/-2 | |
| Tensile Modulus | 13.5 GPa | 1960 ksi | conditioned; ISO 527-1/-2 |
| 19.0 GPa | 2760 ksi | dry; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 9.10 J/cm² | 43.3 ft-lb/in² | dry; ISO 179/1eU |
| 9.60 J/cm² | 45.7 ft-lb/in² | conditioned; ISO 179/1eU | |
| 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
| Charpy Impact, Notched | 1.60 J/cm² | 7.61 ft-lb/in² | dry; ISO 179/1eA |
| 2.60 J/cm² | 12.4 ft-lb/in² | conditioned; ISO 179/1eA | |
| 1.10 J/cm² @Temperature 30.0 °C |
5.23 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
| 1.20 J/cm² @Temperature 30.0 °C |
5.71 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
| Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
| Maximum Service Temperature, Air | 130 - 150 °C | 266 - 302 °F | long term; EMS |
| 200 °C | 392 °F | short term; EMS | |
| Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75-1/-2 |
| Deflection Temperature at 8.0 MPa | 190 °C | 374 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB | HB | IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | conditioned; IEC 60093 |
| 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | dry; IEC 60093 | |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Strength | 33.0 kV/mm | 838 kV/in | conditioned; IEC 60243-1 |
| 36.0 kV/mm | 914 kV/in | dry; IEC 60243-1 | |
| Comparative Tracking Index | 475 V | 475 V | conditioned; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive | Interior | |
| Powertrain and Chassis | ||
| Electricals & Electronics | Connectors | |
| Electrical appliances | ||
| Electrical equipment | ||
| Form | Granules | |
| Industry & Consumer goods | Housewares | |
| Mechanical Engineering | ||
| Sports & Leisure | ||
| Tools & Accessories | ||
| Processing | Injection Molding | |
| Product Attributes | Improved flowability and demoulding |