Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Plastcom SLOVAMID 6 GF 30 FRG 4 LW PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
Kingfa JH820 Modified PC Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 1.6mm; ASTM D149 |
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
Kolon SPESIN® KP270BL General Purpose PBT Compound Resin Excellent waterproofnessApplications: ConnectorsInformation provided by API-Kolon. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.00 mm |
711 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Dielectric Strength | 28.0 - 30.0 kV/mm | 711 - 762 kV/in | DIN 53481 |
Isoflon PC Polycarbonate Good impact resistance among transparent materialsInformation provided by Isoflon. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® T 40 ZS 000000 Partially aromatic polyamide Partially aromatic polyamide, injection molding and extrusion grade, easy release, transparent in all wall thicknesses, isotropic shrinkage, mechanical and electrical properties largely unaffected b.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
Lanxess Pocan® KL 1-7033 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, impact modified |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
Dielectric Strength | 28.0 kV/mm @Thickness 1.60 mm |
711 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50 Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT) 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | |
ExxonMobil Vacmul 3 A Vacmul 3 A is a non-staining, low-viscosity mineral oil, intended for use as an EDM fluid or as a light- to moderate-duty honing oil. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | 50%RH; IEC 60243-1 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Dielectric Strength | >= 28.0 kV/mm | >= 711 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |
|||
Dielectric Strength | 28.0 kV/mm | 711 kV/in | ASTM D149 |
PolyOne Geon™ Vinyl Wire & Cable W9200 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |