Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber FeaturesChemically reinforced with 50% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A70 G50 HW SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | 90.0 - 105 kV/mm | 2290 - 2670 kV/in | Air, 0.125mm Thk Tape; ASTM D149 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | IEC 60250 |
Polyram PlusTek PA301G2 Nylon 6.6 for Injection Molding, 10% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 10% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA301G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA301G50 Nylon 6.6, Heat Stabilized, 50% Glass Fiber Heat stabilized, 50% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA303G43 Nylon 6.6, 43% Glass Fiber 43% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber 50% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | IEC 60250 |
Polyram PlusTek PA303G6BK16 Nylon 6.6, 30% Glass Fiber reinforced, Heat Stabilized, Hydrolysis Resistant 30% Glass fiber reinforced, heat stabilized, hydrolysis resistant, improved surface finish Nylon 6.6. Approved and listed by W.R.A.S.Information provided by Polyram. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA305G6 Nylon 6.6, 30% Glass Fiber Heat stabilized, improved surface quality, 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber 15% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA860 Nylon 6.6, Impact Modified Super tough - impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA865G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA870G33 Nylon 6.6, 33% Glass Fiber 33% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | IEC 60250 |
Polyram PlusTek RA331G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced 30% Glass-fiber reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek RA843 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek RA844 Nylon 6.6, UV Stabilized Impact modified, UV and heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek PA840G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | IEC 60250 |
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | IEC 60250 |
Polyram PlusTek RA303G33 Nylon 66 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 33% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek RA303G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | VDE 0303/4 |
Polyram PlusTek RA303G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized, and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 90.0 - 105 kV/mm | 2290 - 2670 kV/in | Air, 0.125mm Thk Tape; ASTM D149 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | ASTM D149, IEC 243 |
EPICHEM Epinyl PA 6 Polyamide 6 Characteristics: medium viscosity, good mechanical properties |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | ASTM D149, IEC 243 |
EPICHEM PA 6 Polyamide 6 Characteristics: medium viscosity, general purpose |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | |
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided .. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | |
BASF Luranyl® KR 2452/3 Polyphenylene Ether + Styrene-Butadiene Blend This grade, which contains a halogen-free flame-retardant, is especially resistant to heat deformation. Applications include: functional electrical parts (e.g. switches, transformer housings, defle.. |
|||
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | |
BASF Luranyl® KR 2450/3 Polyphenylene Ether + Styrene-Butadiene Blend Easy-flowing grade containing halogen-free, flame-retardant. Uses include: housings for electrical appliances, tubular wiring conduits, tachograph housings.Data was collected by ISO methods and pro.. |