Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | ISO 60243 |
Polikim POLITAL® Polyoxymethylene (POM) Polital® is completely resistant to solvents, petroleum products, oil and grease. It is not resistant to strong acids, bases and oxidants. As it is affected by UV rays, its use in open air is not r.. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | ISO 60243 |
Polikim Polypropylene Polypropylene is an olefin class plastic with low density. It has good chemical and electrical properties and is rigid. Its use under 0°C is not recommended as its mechanical properties weaken. Nor.. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | IEC 60243-1 |
PolyOne Bergamid™ A700 TM-YF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Dielectric Strength | >= 55.1 kV/mm | >= 1400 kV/in | Short Term; 10 mil film; ASTM D149 |
ScanTube PTFE Tubing Information provided by ScanTube, Inc. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | VDE 0303/4 |
Polyram PlusTek RD101 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | VDE 0303/4 |
Polyram PlusTek RD104 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Dielectric Strength | >= 55.0 kV/mm | >= 1400 kV/in | IEC 243; DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 15 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 7 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50 Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and.. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LVX-50H nat PA12-GF50 Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil HDPE HPA 020 Wire & Cable High Density Polyethylene Resin Product Description: HPA 020 is a HDPE grade for Medium/High Voltage power cable jacketing. The grade should be used in blends with LLDPE to improve ESCR. Sufficient Carbon Black or UV stabilizer sh.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin (European Grade) Product Description: LD 100BW is a LDPE containing low antioxidants suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house com.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil LLDPE LL 1002YB Wire & Cable Linear Low Density Polyethylene Resin Product Description: LL 1002YB is a C4 Ziegler Natta LLDPE for Low Voltage power cable and Telecom jacketing. The grade contains a higher level of antioxidants and has excellent Environmental Stress.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
ExxonMobil LLDPE LL 4004EL Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 4004EL is a C4 Ziegler Natta LLDPE, especially designed for Low Voltage power cable insulation, using the two-step silane cross-linking process. Sufficient Cu-inhibitor shoul.. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | |
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | |
Arkema Group Rilsan® BMN Y TLD Nylon 11, MoS2 Filled (Conditioned) Designation ISO 1874-PA11,MHLR,12-020,MD05Rigid grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold release agent.No need of lubricant. L.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | IPC TM-650 2.5.6.2 |
Arlon 35N Fast Cure Polyimide Laminate and Prepreg High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | IPC TM-650 2.5.6.2 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Conditioned) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Dielectric Strength | 55.1 kV/mm @Thickness 0.279 mm |
1400 kV/in @Thickness 0.0110 in |
ASTM D149 |
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
Arlon 32980R015 0.015" (0.381 mm) Uncured Silicon Rubber on Polyester Film Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmProduct Use: Flexible heater substrateAppearance: Red colored, high viscosity gum on polymer liners.. |
|||
Dielectric Strength | 55.0 kV/mm | 1400 kV/in | |