Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polikim Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polikim Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene is an olefin class plastic with low density. It has good chemical and electrical properties and is rigid. Its use under 0°C is not recommended as its mechanical properties weaken. Normally, polypropylene is used in the +0°C, +100°C temperature interval. It is popular in engineering, chemical and electrical industries. Its widest application area is the production of storage tanks, their components and equipment. Polypropylene tanks are preferred in the storage of chemical materials, in water purification and waste management systems.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Water Absorption at Saturation 0.10 %
0.10 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength, Ultimate 29.4 MPa
4270 psi
ISO 527
Elongation at Break >= 50 %
>= 50 %
ISO 527
Tensile Modulus 1.25 GPa
181 ksi
ISO 527
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear 160 µm/m-°C
88.9 µin/in-°F
ISO 11359
Maximum Service Temperature, Air 100 °C
212 °F
continuous
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 55.0 kV/mm
1400 kV/in
ISO 60243
Copyright © lookpolymers.com All Rights Reserved