Arkema Group Rilsan® BMN Y TLD Nylon 11, MoS2 Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 11
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® BMN Y TLD Nylon 11, MoS2 Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA11,MHLR,12-020,MD05Rigid grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold release agent.No need of lubricant. Low friction coefficient. Abrasion resistance. Outstanding mechanical properties. Easy filling of the mold due to its well adapted melt viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption).UL classification: UL94 V2 (3,05mm) RTI(C) 105/90/105Example applications: Moving mechanical parts with friction such as gear or bearing.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Melt Flow 36.2 g/10 min

@Load 2.16 kg,
Temperature 235 °C
36.2 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 18 %
18 %
50 mm/min
Tensile Modulus 1.42 GPa
206 ksi
1 mm/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Melting Point 183 °C
361 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Vicat Softening Point 162 °C
324 °F
50°C/hr; 50N
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 55.0 kV/mm
1400 kV/in
Comparative Tracking Index 600 V
600 V