Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Z Direction, 50% RH; IPC-TM-650 2.5.6.2 |
Rogers Corporation RO4450B Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Z Direction, 50% RH; IPC-TM-650 2.5.6.2 |
Rogers Corporation RO4450F Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC-TM-650.2.5.6.2 |
Park Electrochemical Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Dielectric Strength | 39.4 - 78.7 kV/mm @Thickness 0.0762 mm |
1000 - 2000 kV/in @Thickness 0.00300 in |
|
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Dielectric Strength | >= 39.4 kV/mm | >= 1000 kV/in | DC |
Gwent Electronic Materials D2121102P1 UV Curable Dielectric Ink Screen printable UV cured green dielectric ink with good printability and excellent flexibility. Provides excellent screen life and is suitable for use with automated reel to reel, semi-automatic or.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Dielectric Strength | >= 39.4 kV/mm | >= 1000 kV/in | At 20 mils; ASTM D149 |
Borealis Borstar® ME6053 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar ME6053 is a natural, bimodal medium-density polyethylene compound produced using the Borstar process. It is characterized by its tailor made properties important in jacketing applications, .. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Standard Condition; ASTM D1000 |
3M 1400 Economy Vinyl Electrical Tape 3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chlor.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg 49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | Arlon SQA-TMS-020 |
Arlon 99570R010 0.010" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 14 mil coating; ASTM D149 |
3M Scotchcast™ 260 8 G Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 14 mil coating; ASTM D149 |
3M Scotchcast™ 260 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 15 mil coating; ASTM D149 |
3M Scotchcast™ 262 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 262 is a widely used, well-known general purpose epoxy powder resin. A one-part, red pigmented, rapid heat-curing product, it is designed to provide a continuous, toug.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 15 mil coating; ASTM D149 |
3M Scotchcast™ 263 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 263 is a widely used, well-known general purpose epoxy powder resin. A one part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | |
Astro Met Macor® Machinable Glass Ceramic General Description:Macor is a machinable glass-ceramic material with a unique combination of useful properties. A product of Corning Incorporated, it is stocked, distributed and fabricated by Astro.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon 51N Lead-Free Compatible Epoxy Low-Flow 51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 35% RH |
3M Novec™ 1700 Electronic Grade Coating 3M™ Novec™ 1700 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 2 wt% fluorochemical acrylic.. |
|||
Dielectric Strength | 39.4 kV/mm @Thickness 0.127 mm |
1000 kV/in @Thickness 0.00500 in |
Cured; ASTM D149 |
Aptek DAT-A-THERM 1000 Electrically insulating urethane film DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s.. |
|||
Dielectric Strength | 39.4 kV/mm @Thickness 2.54 mm |
1000 kV/in @Thickness 0.100 in |
|
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | 12 to 14 mil coating; ASTM D149 |
3M Scotchcast™ 260 CG Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon 44981R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene UL Recognition File: E54153.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | ASTM D149 |
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc.. |
|||
Dielectric Strength | 39.4 kV/mm | 1000 kV/in | IPC TM-650 2.5.6.2 |
Arlon 47N Quick Cure Epoxy Low-Flow Prepreg 47N is a low-flow epoxy prepreg engineered for binding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. An optional low lamination temperature protects components already mou.. |