3M Scotchcast™ 262 Electrical Epoxy Powder Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer 3M
Trade Name Scotchcast™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 262 Electrical Epoxy Powder Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M Scotchcast Electrical Resin 262 is a widely used, well-known general purpose epoxy powder resin. A one-part, red pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a variety of substrates.Information provided by 3M
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
cured; ASTM D794
Mechanical Properties Metric English Comments
Impact Test 11.3 J
8.33 ft-lb
12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
Electrical Properties Metric English Comments
Dielectric Strength 39.4 kV/mm
1000 kV/in
12 to 15 mil coating; ASTM D149
Processing Properties Metric English Comments
Cure Time 0.500 min

@Temperature 232 °C
0.00833 hour

@Temperature 450 °F
1.00 min

@Temperature 204 °C
0.0167 hour

@Temperature 399 °F
20.0 min

@Temperature 177 °C
0.333 hour

@Temperature 351 °F
40.0 min

@Temperature 149 °C
0.667 hour

@Temperature 300 °F
Gel Time 0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
hot plate
Shelf Life 24.0 Month

@Temperature <=27.0 °C
24.0 Month

@Temperature <=80.6 °F
Descriptive Properties Value Comments
Appearance Red