Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Muralen® Polyethylene Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from .. |
|||
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 243 |
Quadrant EPP Cestidur™ Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 243 |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
Polymer Industries Polyslick UHMW Sheet Polyslick UHMW Sheet exhibits the properties of excellent impact strength, abrasion resistance, low coefficient of friction, as well as very good chemical resistance. This industrial grade material .. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6) Information provided by PolyOne |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Dielectric Strength | 45.0 kV/mm @Thickness 2.00 mm |
1140 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PE HD Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | VDE 0303 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 243 |
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss Information Provided by LG Chem |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | in air, molded; ASTM D149 |
Guarniflon PTFE G500 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | ASTM D877 |
ExxonMobil 18M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | ASTM D149 |
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | ASTM D877 |
ExxonMobil 13M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PBT Polybutylene Terephthalate The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
ExxonMobil Univis N 32 UNIVIS N hydraulic oils are high-performance anti-wear fluids designed to meet the needs of all major manufacturers and users of hydraulic equipment. They feature high viscosity indexes (VIs), obtai.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30 Product Description: Grilamid LBV-30H FWA natural is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MHL,18-050,GF30Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.Rigidity. High compressive st.. |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |