Polymer Property : Dielectric Strength = 100 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 60243-1
PolyOne Bergamid™ B70 W25 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Dielectric Strength >= 100 kV/mm
>= 2540 kV/in
Grade A
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles)
Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in ..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 60250
Polyram PlusTek PA804 Nylon 6.6 for Injection Molding, Impact Modified
Impact modified Nylon 6.6 for injection molding application.Information provided by Polyram.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PA841 Nylon 6.6, Impact Modified
Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB140 Nylon 6, Injection Molding
Polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 60250
Polyram PlusTek PB142 Nylon 6 for Injection Molding
General purpose, fast cycle Nylon 6 for injection molding applications.Information provided by Polyram.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB150 Nylon 6, Injection Molding
Fast cycle polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB507 Nylon 6, Flame Retardant
Flame retardant halogen free polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB702 Nylon 6, UV Stabilized
Polyamide 6 UV stabilized for fast cycle injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB891 Nylon 6, Impact Modified
Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB145 Nylon 6, Injection Molding
Polyamide 6 for fast cycle injection moldingInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB500 Nylon 6, Flame Retardant
Flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB801 Nylon 6, Impact Modified
impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 60250
Polyram PlusTek PB841 Nylon 6 for Injection Molding, Impact Modified
Impact modified Nylon 6 for injection molding applications.Information provided by Polyram.
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 60250
Polyram PlusTek PB845 Nylon 6 for Injection Molding, Impact Modified
Impact modified Nylon 6 for injection molding applications.Information provided by Polyram.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PB901 Nylon 6, Extruded cable coating
Polyamide 6 for very thin electrical extruded cable coatingInformation provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4
Polyram PlusTek PD100 Nylon 12, Injection Molding
Outstanding polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind.
Dielectric Strength 100 kV/mm
2540 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Hippe PP Polypropylene
Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur B 4300 G2 10% Glass Filled PBT
Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 112
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT
Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic ..
Dielectric Strength 100 - 200 kV/mm
2540 - 5080 kV/in
Thickness up to 1 µm
BACT DLC Diamond-Like Coating
DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and..
Dielectric Strength 100 kV/mm
2540 kV/in
ASTM D149
Solvay Specialty Polymers Algoflon® F3140 X PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT
Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT
Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 243/1
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..