Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS (Asia Pacific) CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 6.60 mm |
>= 120 arcs @Thickness 0.260 in |
UL 746 |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® C2805 PC+ABS LNP* Lubricomp* Cycoloy* C2805 compound is a PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | PLC 0 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | PLC 0 |
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
|
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
|
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
|
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL Rating PLC 0 (>120 arcs) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Asia Pacific) Wear resistant, 7% PTFE filled PC. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics ULTEM LTX300B PEI Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL Rating PLC 0 (>120 arcs) |
Covestro Makrolon® 3105 Polycarbonate Injection molding and extrusion grade with high viscosity, with easy mold release.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and official.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | |
DuPont Teijin Films Mylar® MO21 Polyester Film, 1000 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL Rating PLC 0 (>120 arcs) |
LG Chemical 402 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t.. |