Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.00e+11 - 1.00e+14 ohm | 1.00e+11 - 1.00e+14 ohm | Average value: 2.19e+13 ohm Grade Count:3 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Accelerated; 194°F; 95% RH; 2 days; ASTM D257 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve .. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Accelerated; 194°F; 95% RH; 2 days; ASTM D257 |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Accelerated; 194°F; 95% RH; 2 days; ASTM D257 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Insulation Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control.. |
|||
Insulation Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 80-8387 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Insulation Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 80-8470 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Insulation Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally.. |
|||
Insulation Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S.. |
|||
Insulation Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
IEC 60167 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Dry; IEC 167 |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Wet; 24 hours in water; IEC 167 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Dry; IEC 167 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Insulation Resistance | 1.00e+11 - 1.00e+13 ohm | 1.00e+11 - 1.00e+13 ohm | Dry; IEC 167 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Insulation Resistance | 1.00e+11 ohm @Thickness >=3.00 mm |
1.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i.. |
|||
Insulation Resistance | 1.00e+11 ohm @Thickness >=3.00 mm |
1.00e+11 ohm @Thickness >=0.118 in |
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc.. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Normal; ASTM D257 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Normal; ASTM D257 |
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Normal; ASTM D257 |
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Normal; ASTM D257 |
Chang Chun Plastic Longlite PM T375J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Insulation Resistance | 1.00e+11 - 1.00e+12 ohm @Temperature 90.0 - 90.0 °C |
1.00e+11 - 1.00e+12 ohm @Temperature 194 - 194 °F |
Average value: 5.15e+11 ohm Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Insulation Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Accelerated; 194°F; 95% RH; 2 days; ASTM D257 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |