Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Arc Resistance | 120 sec | 120 sec | ASTM D495 |
Ravago Manufacturing Americas Hylex® P1317L Polycarbonate, UV Stabilized, Higher Flow, Mold Release Information provided by Ravago. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Average value: 150 sec Grade Count:4 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Arc Resistance | 120 sec | 120 sec | Tungsten Electrodes; ASTM D495 |
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
(discontinued **) Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |
|||
Arc Resistance | 120 sec | 120 sec | ASTM D495 |
Kolon KOPA® KN111 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Arc Resistance | 120 sec | 120 sec | ASTM D495 |
Kolon Kopa® KN138R Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | UL Rating PLC 5 (120-180 sec) |
LG Chemical 60HR HIPS Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacu.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 2212EPR PEI 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
SABIC Innovative Plastics Ultem MD130A PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific) 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten, PLC code 5; ASTM D 495 |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
Arc Resistance | 120 sec | 120 sec | ASTM D495 |
Samyang Trirex® 3026PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026PJ is an extrusion grade.Information provided by Samyang. |
|||
Arc Resistance | 120 - 180 sec | 120 - 180 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Arc Resistance | 120 sec | 120 sec | Practical Use (Water Absorption 2.7%); ASTM-D495 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 120 sec | 120 sec | ASTM D495 |
Toyobo T-750 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion gradesInformation provided by Toyobo Co., Ltd |
|||
Arc Resistance | 120 sec | 120 sec | ASTM D495 |
Toyobo T-661 Nylon 66, Standard Grade (DAM) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Arc Resistance | 120 - 180 sec @Thickness 3.00 mm |
120 - 180 sec @Thickness 0.118 in |
UL Rating PLC 5 (120-180 sec) |
Covestro Bayblend® T 64 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Arc Resistance | 120 sec | 120 sec | Tungsten Electrodes; ASTM D495 |
Covestro Makrolon® 2605 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release, Makrolon grade 2658 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Arc Resistance | 120 sec | 120 sec | Tungsten Electrodes; ASTM D495 |
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Arc Resistance | 120 sec | 120 sec | ASTM D495 |
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass Polypropylene provides good resistance to acids, alkalis and organic solvents even at higher temperatures. It is, however, soluble in chlorinated hydrocarbons. Data provided by the manufacturer, Ow.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |