Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D 792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 1.50 - 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.0591 - 0.126 in
SABIC Method
0.0060 - 0.0090 cm/cm

@Thickness 3.20 - 4.60 mm
0.0060 - 0.0090 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm

@Thickness 1.50 - 3.20 mm
0.0050 - 0.0080 in/in

@Thickness 0.0591 - 0.126 in
SABIC Method
0.0080 - 0.011 cm/cm

@Thickness 3.20 - 4.60 mm
0.0080 - 0.011 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D 785
Tensile Strength at Break 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 5.0 %
5.0 %
Type I, 5 mm/min; ASTM D 638
Flexural Strength 144 MPa
20900 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 4.82 GPa
699 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.530 J/cm

@Temperature 23.0 °C
0.993 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm

@Temperature 23.0 °C
10.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 60.0 - 138 °C
12.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
21.6 µm/m-°C

@Temperature -40.0 - 95.0 °C
12.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 210 °C

@Thickness 6.40 mm
410 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 190 °C

@Thickness 6.40 mm
374 °F

@Thickness 0.252 in
unannealed; ASTM D 648
UL RTI, Electrical 130 °C
266 °F
UL 746B
UL RTI, Mechanical with Impact 130 °C
266 °F
UL 746B
UL RTI, Mechanical without Impact 140 °C
284 °F
UL 746B
Flammability, UL94 HB

@Thickness 0.710 mm
HB

@Thickness 0.0280 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 3.30e+16 ohm-cm
3.30e+16 ohm-cm
ASTM D 257
Dielectric Constant 3.4

@Frequency 1.00e+6 Hz
3.4

@Frequency 1.00e+6 Hz
ASTM D 150
3.6

@Frequency 100 Hz
3.6

@Frequency 100 Hz
ASTM D 150
Dielectric Strength 19.6 kV/mm

@Thickness 3.20 mm
498 kV/in

@Thickness 0.126 in
in air; ASTM D 149
23.2 kV/mm

@Thickness 1.60 mm
589 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
Dissipation Factor 0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
ASTM D 150
0.020

@Frequency 1.00e+6 Hz
0.020

@Frequency 1.00e+6 Hz
ASTM D 150
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten, PLC code 5; ASTM D 495
Comparative Tracking Index 250 - 400 V
250 - 400 V
PLC code 2; UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
PLC code 1; UL 746A