Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene .. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Plenco 51045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Arc Resistance | 80 sec | 80 sec | Dry; ASTM D495 |
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Arc Resistance | 80 sec | 80 sec | Dry; ASTM D495 |
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Arc Resistance | 80 sec | 80 sec | Dry; ASTM D495 |
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Unitika AXF-1500-05 Conditioned Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Toyobo Vylopet® EMC605 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanic.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Toyobo Vylopet® EMC615 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: electrical and electronic componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Toyobo Vylopet® EMC630 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
Arc Resistance | 80 sec | 80 sec | across filaments; 50% RH and at 90% RH |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 540V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 540Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 100Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® X9102 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Arc Resistance | 80 sec | 80 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Plenco 51015 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |
|||
Arc Resistance | 80 sec | 80 sec | ASTM D495 |
Plenco 51015 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |