Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 20%Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengthGood dimensional stabilityGood resistance to hydrolysis and sterilizationGood oxidative stabilityInherent flame retardanceApplications: Reusable hypodermic syringesSurgical instruments and componentsPrinted circuit boardsCircuit breaker componentsOil level indicatorsHeat exchanger partsEngine componentsHousehold appliancesFilter housingsSanitary and pipe fittingsInformation provided by Gharda.Solvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Filler Content 20 %
20 %
Moisture Absorption at Equilibrium 0.30 %
0.30 %
ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527
Flexural Strength 175 MPa
25400 psi
ISO 178
Flexural Modulus 6.50 GPa
943 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 185 °C
365 °F
Continuous use
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75
Glass Transition Temp, Tg 225 °C
437 °F
DSC
Flammability, UL94 V-0
V-0
Oxygen Index 41 %
41 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
IEC 93
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 93
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 243/1
Arc Resistance 80 sec
80 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
IEC 112