Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data) Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data) Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data) FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data) Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |