Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Arnite® TV4 460 KL TV4 460 PBT/PET Blend-30% Glass Reinforced (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 24 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 27 U Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® FC 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® FC 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC407 Non-Reinforced Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessImproved processabilityHigh fluidityGood appearanceInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Arnite® TV4 260 S PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.05 mm |
250 - 399 V @Thickness 0.120 in |
UL PLC 2 (250-399 V) |
Resinoid 1312 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® C CM 506 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |