Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® 923 PC Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific) Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® 943AR PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® FL910 PC Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm). |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® FL920 PC Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific) 10 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East) Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | PLC code 3; UL 746A |
SABIC Innovative Plastics Lexan® PPC4701 PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Comparative Tracking Index | 175 - 250 V @Thickness 3.05 mm |
175 - 250 V @Thickness 0.120 in |
UL PLC 3 (175-250 V) |
Resinoid 7051 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | PLC code 3; UL 746A |
SABIC Innovative Plastics Cycoloy® FXC810MA PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810MA is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require marble colour effects. The colour package may effect performance.This data was suppl.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746 |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific) Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | Average value: 213 V Grade Count:3 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | PLC code 3; UL 746A |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | PLC code 3; UL 746A |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Valox® 457 PBT 6.5% GR PBT, UL94 V-0/5V. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA 10% Glass Reinforced PPE+PA Alloy. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Comparative Tracking Index | 175 - 250 V @Thickness 0.750 mm |
175 - 250 V @Thickness 0.0295 in |
UL 746A |
DuPont Performance Polymers Crastin® SK692FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |