Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Comparative Tracking Index | 550 V | 550 V | CTI-M 100; IEC 112 |
Nilit FRIANYL A63 E Raw extruded nylon 6.6 for injection molding Raw extruded nylon 6.6 for injection molding (available only in nature).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 KV25 Nylon 6 for injection molding, 25% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | |
Radici Radilon® S CP300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 HS-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | CTI 100; IEC 112 |
Nilit FRIANYL C73 HS-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 550 V | 550 V | |
Radici Radilon® S RCV3015 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Comparative Tracking Index | 550 V | 550 V | A solution |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Comparative Tracking Index | 550 V | 550 V | CEI 112 |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Comparative Tracking Index | 550 V | 550 V | Solution A; IEC 60112 |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Comparative Tracking Index | 550 V | 550 V | UL 746 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Comparative Tracking Index | 550 V | 550 V | IEC Method |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6600 GV 35 HWCP 35% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | Stufe; IEC 112 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |
Addiplast Addinyl B2 V50 Nylon 6, 50% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |
Addiplast Addinyl B2 ZV 50 Nylon 6, 50% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Comparative Tracking Index | 550 V | 550 V | Test solution A; IEC 60112 |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Comparative Tracking Index | 550 V | 550 V | Test solution A; IEC 60112 |
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 593 V Grade Count:5 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Comparative Tracking Index | 550 V | 550 V | dry; IEC 60112 |
DSM Novamid® 3021GH30 BK629 PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Comparative Tracking Index | 550 V | 550 V | IEC 60112 |
DSM Akulon® K220-HGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Dry)
(discontinue The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 550 V | 550 V | |
Plastcom SLOVASTER® B2 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Comparative Tracking Index | 550 V | 550 V | Test Liquid A; IEC 60112 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |
|||
Comparative Tracking Index | 550 V | 550 V | UL 746 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Comparative Tracking Index | 550 V | 550 V | GB/4207 |
Zhejiang Juner PA-A6-6H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide Applications: Circuit Breaker, BaseInformation provided by Zhejiang Juner New Materials Co, Ltd. |