Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Qualchem Danamid FES-23 HUV Polyamide 6 Impact resistant, cold. Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial light.Information provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Qualchem Danamid FES-23 Polyamide 6 Impact resistant, coldInformation provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Comparative Tracking Index | 525 - 600 V | 525 - 600 V | Average value: 588 V Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 525 - 600 V | 525 - 600 V | Average value: 586 V Grade Count:61 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
LG Chemical RS-650 ABS, Extrusion, General Purpose Information Provided by LG Chem |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
Comparative Tracking Index | 525 V | 525 V | d.a.m.; Solution A; IEC 60112 |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution A; IEC 60112 |
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer.. |
|||
Comparative Tracking Index | 525 V | 525 V | Solution B; IEC 60112 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Comparative Tracking Index | 525 V | 525 V | ASTM D3638 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Comparative Tracking Index | 525 V | 525 V | GB4207 |
Zhejiang Juner PA-A6 GF20% Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Comparative Tracking Index | 525 V | 525 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced 20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Comparative Tracking Index | 525 V | 525 V | Test solution A; IEC 112 |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Comparative Tracking Index | 525 V @Thickness 3.00 mm |
525 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 112 |
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Comparative Tracking Index | 525 V | 525 V | IEC 60112 |
Lanxess Pocan® DP B 3235 XF 901510 PBT, 30% Glass Fiber
(discontinued **) PBT, 30% glass fibers, injection molding, improved flowability |