Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
SABIC Innovative Plastics Lexan® 201 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746 |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Comparative Tracking Index | >= 250 V | >= 250 V | CTI; IEC 60112 |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Comparative Tracking Index | 250 - 350 V | 250 - 350 V | Average value: 308 V Grade Count:12 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
SABIC Innovative Plastics Lexan® 945A PC (Europe-Africa-Middle East) Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC 2 |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC 2 |
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Comparative Tracking Index | 250 - 600 V | 250 - 600 V | Average value: 502 V Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Comparative Tracking Index | 250 - 650 V | 250 - 650 V | Average value: 534 V Grade Count:32 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Comparative Tracking Index | 250 V @Thickness 2.00 mm |
250 V @Thickness 0.0787 in |
IEC 112 |
LG Chemical Lupoy 1300-15 Polycarbonate Resin Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Comparative Tracking Index | 250 V @Thickness 2.00 mm |
250 V @Thickness 0.0787 in |
IEC 112 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | Solution A; UL 746A |
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Comparative Tracking Index | 250 V | 250 V | UL 746 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC code 2; UL 746A |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | 250 V @Thickness 2.00 mm |
250 V @Thickness 0.0787 in |
Solution A; IEC 60112 |
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
Polyplastics FR-PET® C9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Comparative Tracking Index | 250 V | 250 V | IEC 60112 |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on pol.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Comparative Tracking Index | 250 V @Thickness 3.20 mm |
250 V @Thickness 0.126 in |
ASTM D3638 |
Beijing Chemical Industry KAIFA® 301-G15RF PBT Resin 15% glass fiber reinforced, flame retardant, good toughness, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Comparative Tracking Index | 250 V | 250 V | CEI 60112/Solution A |
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |