Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 600 V | 600 V | |
Polycasa Acryl® G 77 Acrylic, Injection Molding Grade Injection molding grade for record player covers, optical fibers, display windows, logos, condiment containers, desk organizers.Data was collected by ISO methods.Quinn Manufacturing Group rebranded .. |
|||
Comparative Tracking Index | 600 V | 600 V | ASTM D2303 |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Comparative Tracking Index | 600 V | 600 V | ASTM D2303 |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | CTI; IEC 60112 |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | PLC code 0; UL 746A |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | >= 600 V @Thickness 1.60 mm |
>= 600 V @Thickness 0.0630 in |
|
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Lanxess Durethan® B 31 SK 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Lanxess Pocan® KU 2-7205 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant |
|||
Comparative Tracking Index | 600 V | 600 V | A solution |
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
DSM Akulon® S223-EH Nylon 66 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 600 V | 600 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45 Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST.. |
|||
Comparative Tracking Index | 600 V | 600 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Comparative Tracking Index | 600 V | 600 V | DAM; IEC 60112 |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Comparative Tracking Index | 600 V | 600 V | |
Arkema Group Altuglas® GR 7E LIL Acrylic ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance .. |
|||
Comparative Tracking Index | 600 V | 600 V | |
Arkema Group Orgalloy® RS 6000TLA Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Comparative Tracking Index | 600 V | 600 V | Test solution A; IEC 60112 |
BASF Ultraform® N2650 Z6 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF |
|||
Comparative Tracking Index | 600 V | 600 V | |
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t.. |
|||
Comparative Tracking Index | >= 600 V | >= 600 V | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Comparative Tracking Index | 600 V | 600 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® GV-6H PA*-GF60 Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
DSM Arnite® T06 204 XL PBT Low Viscosity, Injection Molding, Low outgassing |
|||
Comparative Tracking Index | 600 V | 600 V | dry; IEC 60112 |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
Comparative Tracking Index | 600 V | 600 V | Conditioned; UL 746 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |