Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade , Nylon, Aromatic
Manufacturer Arkema
Trade Name Cristamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good thermal resistance. Sterilizable. Dimensional stability.USP XXIII class VI approval.Example applications: Catheters.ISO data provided by the manufacturer, Arkema.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.0 MPa
10300 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 7.0 %
7.0 %
50 mm/min
Tensile Modulus 2.08 GPa
302 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 0.820 J/cm²
3.90 ft-lb/in²
0.250 J/cm²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Dielectric Strength 50.0 kV/mm
1270 kV/in
Comparative Tracking Index 600 V
600 V