Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 575 V | 575 V | |
Plastcom SLOVAMID 66 GF 50 LS PA66, 50% glass fibre, light stability FeaturesChemically reinforced with 50% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry, l.. |
|||
Comparative Tracking Index | 575 V | 575 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 SG-GV20 Nylon 6 for injection molding, 20% glass fiber reinforced Nylon 6 for injection molding, light impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 575 V | 575 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 W-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | >= 575 V | >= 575 V | CTI; IEC 60112 |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Comparative Tracking Index | 575 V | 575 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 GV20 Nylon 6 for injection molding, 20% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 575 V | 575 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 575 V | 575 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 H-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 575 V | 575 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 W-KV10 Nylon 6 for injection molding, 10% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 575 V | 575 V | IEC 112 |
LG Chemical RS-800 ABS, Extrusion, High Impact, HCFC Resistant Information Provided by LG Chem |
|||
Comparative Tracking Index | 575 V | 575 V | IEC 112 |
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss Information Provided by LG Chem |
|||
Comparative Tracking Index | 575 V | 575 V | IEC 60112 |
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1 |
|||
Comparative Tracking Index | 575 V | 575 V | Solution B; IEC 60112 |
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Comparative Tracking Index | 575 V | 575 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® GV-2 FWA nat PA*-GF20 Product description: Grivory GV-2 FWA natural is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyami.. |
|||
Comparative Tracking Index | 575 V | 575 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35 Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Comparative Tracking Index | 575 V | 575 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15 Information provided by EMS Grivory |
|||
Comparative Tracking Index | 575 V | 575 V | IEC 60112 |
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight w.. |
|||
Comparative Tracking Index | 575 V | 575 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® BG-50 PA6-GF50 Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su.. |
|||
Comparative Tracking Index | 575 V | 575 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Comparative Tracking Index | 575 V | 575 V | IEC 60112 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 575 V | 575 V | Test Solution A; IEC 60112 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
Comparative Tracking Index | 575 V | 575 V | IEC 60112 |
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Comparative Tracking Index | 575 V | 575 V | IEC 60112 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Comparative Tracking Index | 575 V | 575 V | Conditioned; IEC 60112 |
Solvay Technyl® A 402 H1 Nylon 66 Unreinforced, very high viscosity, heat stabilized, for extrusion and injection molding. TECHNYL® A 402 H1 offers three main advantages: high impact resistance at low humidity levels, good rigidit.. |