Material Notes:
This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.50 %
0.50 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 1.0 %
1.0 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 64.0 MPa
9280 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 25.0 MPa
3630 psi
v = 50 mm/min; ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Tensile Modulus 0.400 GPa
58.0 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched NB
NB
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 171 °C
340 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 75.0 °C
167 °F
Long Term
125 °C
257 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 125 - 165 °C
257 - 329 °F
ISO 75-2
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 31.0 kV/mm
787 kV/in
in transformer oil; IEC 60243-1
Comparative Tracking Index 575 V
575 V
IEC 60112