Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 100 ohm @Thickness 0.400 mm |
<= 100 ohm @Thickness 0.0157 in |
ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Faradex MS003XXC PP (Europe-Africa-Middle East) LNP* Faradex* MS003XXC is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This data was supplied by SABIC-IP for.. |
|||
Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | 100 ohm | 100 ohm | ASTM D4496 |
LNP Lubricomp® ECL-4036 Polyetherimide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D4496 |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Surface Resistance | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |
Techmer ES Electrablend® ABS 03007 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS (Asia Pacific) LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Surface Resistance | 100 - 200 ohm | 100 - 200 ohm | ASTM D257 |
Techmer ES Electrablend® PA6/6 CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Surface Resistance | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Surface Resistance | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON WC003 PBT (Europe-Africa-Middle East) LNP* Stat-kon* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON WE002 PBT LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East) LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive. |
|||
Surface Resistance | 100 ohm | 100 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon WX98547 PBT LNP* Stat-kon* WX98547 is a compound based on Polybutylene Terephalate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SAB.. |
|||
Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon DE0049 PC (Europe-Africa-Middle East) LNP* Stat-kon* DC-1004 FR is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.This.. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |
Techmer ES Electrablend® PC SS15 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |