Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | STN IEC 60093 |
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO.167 DN.53482 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300 PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | E - 24/125; IPC-TM-650.2.5.17.1 |
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IPC-TM-650.2.5.17 |
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Appl.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+14 ohm | 1.00e+13 - 1.00e+14 ohm | |
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
GEHR Plastics PA 6 C Nylon 6 Cast Very stressed-relieved and high-molecular weight PA6.Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be ac.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | cond.; IEC 60093 |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | DIN 53482 |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | DIN 53482 |
Polyram PlusTek PB702 Nylon 6, UV Stabilized Polyamide 6 UV stabilized for fast cycle injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ISO IEC 93 |
Total Polystyrene Impact 8260 Improved Environmental Stress Crack Resistance High Impact Polystyrene POLYSTYRENE IMPACT 8260 is a high impact polystyrene for extrusion and injection applications. This grade has an improved environmental stress crack resistance in comparison with standard high impa.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
DSM Akulon® M-1016 (Cond.) 33% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NA40 NL E PA 6.6 lubricated, nucleated Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NB40 NL E PA 6 lubricated, nucleated Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NA40 GR15 NL XA 20 PA 6.6 15% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | Conditioned; CEI 60093 |
Addiplast Addilene J 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | |
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 93 |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering .. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | Conditioned; CEI 60093 |
Addiplast Addilene H 490 M40F Flame Retardant Polypropylene, 40% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® Nb40 GR30 NL PA6, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
CENTROPLAST CENTRO HPM Polyphenylensulfone This plastic has very good mechanical, electrical and thermal properties. It has very good hydrolysis resistance, and is suitable for medical, and pharmaceutical equipment construction.Information .. |
|||
Surface Resistance | 1.00e+13 - 3.00e+15 ohm | 1.00e+13 - 3.00e+15 ohm | Average value: 4.48e+14 ohm Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |