Material Notes:
This plastic has very good mechanical, electrical and thermal properties. It has very good hydrolysis resistance, and is suitable for medical, and pharmaceutical equipment construction.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.60 %
0.60 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 1.2 %
1.2 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80

@Thickness 10.0 mm
80

@Thickness 0.394 in
ISO 2039-2
Tensile Strength, Yield 76.0 MPa
11000 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 10 %
10 %
ISO 527-2
Tensile Modulus 2.50 GPa
363 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 180 °C
356 °F
Long Term
210 °C
410 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-2
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.4

@Frequency 100 Hz
3.4

@Frequency 100 Hz
IEC 60250
3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
IEC 60250
0.0050

@Frequency 1e+6 Hz
0.0050

@Frequency 1e+6 Hz
IEC 60250