Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 1.00e+10 ohm @Thickness 3.00 mm |
<= 1.00e+10 ohm @Thickness 0.118 in |
molded plate; ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 7300 PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | IEC 60093 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Hexion Bakelite™ PF 14600 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, low specific gravity.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a part of Hexion in 2005.. |
|||
Surface Resistance | >= 1.00e+10 ohm | >= 1.00e+10 ohm | |
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | cond.; IEC 60093 |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | DIN 53482 |
Schwartz Technical Plastics LAMIGAMID® 310 Cast Polyamide 6, Conditioned Application: sheaves, wheels, rollers, mandrell segments, coupling parts, vibrator parts etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | DIN 53482 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | DIN 53482 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ASTM D257 |
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer Description: Stat-Rite® E-1140 is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1140 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to .. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | DIN 53482 |
Polyram PlusTek PB320G6 Nylon 6, 30% Glass Fiber, Flame Retardant 30% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+10 - 3.00e+10 ohm | 1.00e+10 - 3.00e+10 ohm | DIN 53482 |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
EMS-Grivory Grivory® BK-50 PA6-GB50 Information provided by EMS Grivory |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 GV 15 HWCP 15% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000/58 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6600 MR 209 HWCP 20% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6600/50 GV 15 HWCP 15% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Conditioned, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | |
BASF Gusspolyamid® Nylon 6 (At 50% RH) Processed by anionic polymerization of caprolactam in the presence of a catalyst and activator. Uses include semi-finished products and containers (e.g. heating oil tanks).Data was collected by ISO.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) Information provided by BASF |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Conditioned, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 5.72e+14 ohm Grade Count:40 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | |
BASF Novolen® 1148 TC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |