Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 7.69e+14 ohm Grade Count:9 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | Average value: 5.50e+15 ohm Grade Count:4 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 2.33e+15 ohm Grade Count:13 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Surface Resistance | 100 - 1.00e+16 ohm | 100 - 1.00e+16 ohm | Average value: 1.24e+15 ohm Grade Count:22 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 1.00e+9 - 1.00e+16 ohm | 1.00e+9 - 1.00e+16 ohm | Average value: 1.03e+15 ohm Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | Average value: 6.70e+15 ohm Grade Count:3 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | ASTM D 257 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Surface Resistance | 10000 - 1.00e+16 ohm | 10000 - 1.00e+16 ohm | Average value: 3.92e+15 ohm Grade Count:26 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Surface Resistance | 10000 - 1.00e+16 ohm | 10000 - 1.00e+16 ohm | Average value: 2.17e+15 ohm Grade Count:26 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | Average value: 4.67e+15 ohm Grade Count:27 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Surface Resistance | 2000 - 1.00e+16 ohm | 2000 - 1.00e+16 ohm | Average value: 8.84e+14 ohm Grade Count:35 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+16 ohm | 1.00e+9 - 1.00e+16 ohm | Average value: 8.68e+14 ohm Grade Count:29 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 2.51e+15 ohm Grade Count:4 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 1.30e+15 ohm Grade Count:33 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | Average value: 4.56e+15 ohm Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 3.07e+15 ohm Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 7.47e+14 ohm Grade Count:31 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 3.60e+14 ohm Grade Count:36 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 4.36e+14 ohm Grade Count:23 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 8.14e+14 ohm Grade Count:69 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Surface Resistance | 1.00 - 1.00e+16 ohm | 1.00 - 1.00e+16 ohm | Average value: 9.40e+14 ohm Grade Count:113 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 5.11e+14 ohm Grade Count:20 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | ASTM D257 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | ASTM D257 |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+16 ohm | 1.00e+14 - 1.00e+16 ohm | ASTM D257 |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |
|||
Surface Resistance | 1.00e+15 - 1.00e+16 ohm @Temperature 23.0 °C |
1.00e+15 - 1.00e+16 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers VESPEL TP-8161 Polyimide DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environm.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+16 ohm | 1.00e+10 - 1.00e+16 ohm | Average value: 8.03e+14 ohm Grade Count:15 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Surface Resistance | 1.00e+6 - 1.00e+16 ohm | 1.00e+6 - 1.00e+16 ohm | Average value: 1.70e+15 ohm Grade Count:20 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Surface Resistance | 100 - 1.00e+16 ohm | 100 - 1.00e+16 ohm | Average value: 2.50e+14 ohm Grade Count:58 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Surface Resistance | 1000 - 1.00e+16 ohm | 1000 - 1.00e+16 ohm | Average value: 2.82e+15 ohm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |