Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00 - 1.00e+6 ohm-cm | 1.00 - 1.00e+6 ohm-cm | Average value: 270000 ohm-cm Grade Count:35 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | Average value: 21.1 ohm-cm Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1.00 ohm-cm - 1e+05 | 1.00 ohm-cm - 1e+05 | Average value: 180 ohm-cm Grade Count:16 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 1.00 - 2.00e+13 ohm-cm | 1.00 - 2.00e+13 ohm-cm | Average value: 1.25e+12 ohm-cm Grade Count:18 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | Average value: 21.3 ohm-cm Grade Count:6 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Electrical Resistivity | 1.00 - 1.00e+16 ohm-cm | 1.00 - 1.00e+16 ohm-cm | Average value: 1.16e+15 ohm-cm Grade Count:126 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 1.00 - 1.00e+17 ohm-cm | 1.00 - 1.00e+17 ohm-cm | Average value: 2.93e+15 ohm-cm Grade Count:243 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00 - 1.00e+13 ohm-cm | 1.00 - 1.00e+13 ohm-cm | Average value: 4.17e+11 ohm-cm Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Electrical Resistivity | 1.00 - 10000 ohm-cm | 1.00 - 10000 ohm-cm | Average value: 699 ohm-cm Grade Count:23 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | |
A. Schulman ComAlloy E-16901B PPS Alloy, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 1.00 - 1.00e+16 ohm-cm | 1.00 - 1.00e+16 ohm-cm | Average value: 8.55e+14 ohm-cm Grade Count:156 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Electrical Resistivity | 1.00 ohm-cm - 1e+05 | 1.00 ohm-cm - 1e+05 | Average value: 118 ohm-cm Grade Count:9 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Electrical Resistivity | 1.00 - 10000 ohm-cm | 1.00 - 10000 ohm-cm | Average value: 1690 ohm-cm Grade Count:7 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Electrical Resistivity | 1.00 ohm-cm - 1e+05 | 1.00 ohm-cm - 1e+05 | Average value: 25.0 ohm-cm Grade Count:10 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Electrical Resistivity | 1.00 - 9.90e+10 ohm-cm | 1.00 - 9.90e+10 ohm-cm | Average value: 2.22e+9 ohm-cm Grade Count:26 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00 ohm-cm | 1.00 ohm-cm | |
Ceradyne CeraTrex™ 146-12E Silicon Carbide Features:corrosion resistancewear resistancetailored electrical propertiesApplications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Electrical Resistivity | 1.00 - 3.10e+9 ohm-cm | 1.00 - 3.10e+9 ohm-cm | Average value: 2.40e+8 ohm-cm Grade Count:16 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |